CMS Pixel Detector
Miscellaneous
|
Phase 1
Phase 2
|
Layer 1 Replacement
Layers 2-4
|
Layer 1 Replacement Elog |
Not logged in |
|
|
Message ID: 269
Entry time: Fri May 22 16:06:43 2020
|
Author: |
Andrey Starodumov |
Category: |
XRay HR tests |
Subject: |
Analysis of HRT: M1623, M1632, M1634, M1636-M1639,M1640 |
|
|
Module HRtest VCal calibration Grade
#defects max #noisy pix
ColdBox XRay
M1623 130 151 91 45xVCal-67e- B
M1630 80 1 385 43xVcal-290e- A
M1632 14 9 124 45xVcal-145e- A
M1634 33 81 339 43xVcal-347e- B
M1636 10 14 109 46xVcal-255e- A
M1637 71 45 175 45xVcal-182e- A
M1638 12 95 269 43xVcal-183e- B
M1639 21 96 482 43xVcal-441e- B
M1640 30 22 115 44xVcal-134e- A |